Connect with
KP Alumni now!

recent registrants


Forums - Reunions - Venues - how to identify composite flooring

how to identify composite flooring

Posted by Wangkiky Wangkiky over 6 months ago

How to identify the floor to teach you to strengthen laminate flooring First of all, to know the identification of indicators to strengthen the floor, but also know that simple and easy identification method. Flooring that: to strengthen the flooring to the extent of today's fake, and government regulation is not strong and consumers do not have the ability to identify, have a great relationship.[url=http://wpcdeckmaterials.com/blog/167.html]Eco Wall Panel System[/url] A few days ago someone also wrote how to choose to strengthen the floor, such as brand, price, origin, wear, formaldehyde, etc., these indicators are good or bad, how consumers can see it? Is not listening to the ad said, listening to vendors say, who said nice to buy the floor. Strengthen the floor of the most critical test indicators are four: formaldehyde emission, wear-resistant surface, the thickness of water swelling and floor geometry. 1, the determination of formaldehyde emission: [url=http://wpcproduct.com/blog/custom-size-wood-plastic-fence.html]Custom size wood-plastic fence[/url] the choice of good sealing performance of the big mouth bottles, saw the same size of several alternative brands of the model, into different bottles, sealed 24 hours, open the bottle, one by one smell, you will compare Out, which brand of formaldehyde emission of the floor is small. If the fear is not accurate, you can two people, has heard the news, more sure. 2, the surface wear level: with 180 sandpaper (sandpaper thickness, the problem is not), the same person, with the same strength and law, continuous friction floor with the same ground, 50 times. There is no aluminum oxide on the floor, it is likely that [url=http://wpcproduct.com/blog/low-water-absorption-rate-composite-wood-floor.html]Low Water Absorption Rate Composite Wood Floor[/url] the grain of paper will be severely damaged. Wear-resistant paper on the floor, the surface will not have a serious scratch; or lower grams of wear-resistant paper, the surface will have different degrees of wear and tear. 3, the thickness of water swelling: Saw the approximate size of the alternative model, number, into the boiling water, 5-8 minutes. Out to compare the degree of expansion of their edges.[url=http://wpcproductsupplier.com/blog/professional-wpc-supplier-in-china.html]Professional WPC Supplier In China[/url] The best in advance with a micrometer, measuring the thickness of the measuring point of the template to make the mark. After soaking in water, take out and then measure the thickness, can be calculated after boiling water immersion, the relative thickness of the floor water swelling. 4, the floor of the geometric size: This comparison test needs to use the whole board comparison. A) will be two pieces of the floor together, hand-touch the height difference between the joints; in the floor between the model, you can also consciously touch, compare. The difference between brands should be obvious. B) Next look at the tightness of the splice gap. A little floor scoliosis, patchwork will not be very tight. This reflects the machining accuracy of the floor.